Business Type:
Manufacturer/Factory
Establishment:
2012
R&D Capacity:
ODM, OEM, Other
OEM/ODM Service
Sample Available

Normal Dome Lid, Glass Lid, Silicon Glass Lid manufacturer / supplier in China, offering Glass Lid, Normal Dome Tempered Glass Lid for Cookware, Glass Lid, Wide Ring, Tempered Glass Lid, Stainless Steel Knob for Cookware, Pot, Pan Lid and so on.

1
    YRS
General Supplier
Supplier Homepage Light Industry & Daily Use Cookware Cookware Parts 28cm Ez Cooking High Dome Tempered Glass Pan Lid

28cm Ez Cooking High Dome Tempered Glass Pan Lid

Get Latest Price
Min. Order / Reference FOB Price
1000 Pieces US $8.85/ Pieces
Local Area: Taiwan, China
R&D Capacity: OEM, ODM, Other
Payment Terms: LC, T/T, PayPal
Shape: Round
Customized: Customized
Color: Transparent
Product Specification and Features
- Material of tempered glass lid: Float glass
- Stainless Steel rim: SUS304
- Diameter: 28cm
- Thickness: 5mm
- Heat resistance: 300- 320 degree centigrade
- Thermal shock: 150 degree centigrade
- Shape: Round,
- Colors: Clear,
- Sample Terms: Samples are available upon receipt of your requests
- Minimum order quantity: 1000PCS or negotiable
Test for quality control:1. FLATNESS CHECKPlace the glass lid on a completely smooth table , and put a piece of 1mm thickness iron plate beside the ring the glass lid, then moving the iron gauge along with the circumference of the lid, the glass lid passes the test if the iron plate does not push in2. THTERMAL SHOCKPut the glass lid into oven temperature to 200°C, and constant temperature for 30 minutes, remove it immediately into 20°C water , glass no broken or crack3. IMPACT TESTPlace a lid, domed size up, on a hard surface,Dropping a 225 grams steel ball from a height of 1.5meter,No fracture no shatter, to passNote : Don't drop the ball near or onto a vent hole /rivet hole 4. SCRATCH TEST (PRESSURE TEST)Use 120-grit (abrasive paper ) sandpaper to scratch two side and three directions 15 times, then put into room temperature water for 15 minutes, it pass if no breakage and no crack.5. POLOLARISCOPE CHECKTo test the balance of compressive stress and tensile stress depends on the color what you see.6. FRAGMENTATION CHECKApply tape (adhesive film)on the convex (front) surface of the lid, domed side upward, break it with a hammer broken 5X5cm measuring range , number of particles (fragments) counted should be at least 40,The purpose of this test is to determine whether the glass has been adequately toughened.