Business Type:
Manufacturer/Factory
Establishment:
2012
R&D Capacity:
ODM, OEM, Other
OEM/ODM Service
Sample Available

Liquid Filling Machine, Small Water Bottling Machine, Filling Machinery manufacturer / supplier in China, offering Mineral Water Plant Production Line Small Bottle 5L 10L Bottle Washing Filling Capping Labeling Packing Machine, Small Automatic Liquid Paste Packing Machine / Spicy Sauce/Oil Sauce/Condensed Milk Packing Machine, Fruit Juice Ketchup Spicy Sauce Packaging Machine and so on.

1
    YRS
General Supplier

China 30 25 Pet Preform for 500ml Bottle

Get Latest Price
Min. Order / Reference FOB Price
100000 Piece US $0.15/ Piece
Local Area: Shenzhen, Guangdong, China
R&D Capacity: OEM, ODM, Other
Payment Terms: LC, T/T, PayPal
Type: Stretch Blow Molding Machine
Raw Material: PET
Making Method of Parison: Injection Blowing

Pet Beverage/Juice Bottles Hot Filling Preform

Product Description
Our preforms have high reputation in competitive price and high quality. we have many kinds of
preforms which can be blew to botte from 100ml to 5 gallon .
Our preforms are suitable for purified mineral water bottle ,medicine bottle ,beverage bottle ,oil bottle etc .We can produce any kind of preform in according to customer's requirements. Feature :
Our PET Preform Features:
1) 100% new PET resin
2) High transparency
3) High toughness
4) Blowing Rate up to 99.7-99.8%
5) Low Defect Rate
6) a wide range of neck and weight perform
7) Different colors is workable,
8) Open new molds with low cost and less time
9) Competitive price with high quality
10) On time delivery
Hi Charif.It is Sandy from ESAQUA. We are a factory to produce high quality extrusion blowing machine at very competitive price. Pls reply back for best quote, thanks, nice day!

Preform Types&Spec :

preforms for Juice,Tea, CDS,Energy Drink, Milk & Dairy Product BottlesNeck FinishMaterialWeight(g)PCO 1810 28mmPET16 ,18, 21, 23 ,24 ,25 ,27 ,28 ,30 ,31, 35 ,40 ,43 ,50 ,55, 60, 65PCO 1881 28M
PET13, 15, 17, 19 ,21, 23, 24, 25, 27, 30 ,35, 38, 43, 45High Neck 30mmPET12, 13, 14Short Neck 30mmPET14, 15 ,16 ,17, 18, 21, 24 ,25, 26, 28, 30 ,38, 50 Preforms For Edible Oil BottlesNeck FinishMaterialWeight(g)Short Neck 30mmPET150 ,170 ,200 ,230, 240, 250, 270 ,280Preforms For Cosmetic BottleNeck FinishMaterialWeight(g)28 mmPET21, 35 Preforms For 5 Gallon Water BottleNeck FinishMaterialWeight(g)55mmPET350, 440, 530, 650 ,680 ,700 720, 750



Packing& Delivery :
30mm preform as an example
carton size:52.5*32.5*32.5cm
Quantity:610ctns/20GP,1230ctns/40HQ
Delivery time: with 5-7days for MOQ after prepayment /confirm/ied
Payment terms: 30% deposit T/T before production, the balance before shipping.
Package details: inner polybag,export standard outer carton
Remark: above items can be negotiated
TROUBLE SHOOTING BLOWING PROCESS:
Problem : Haze
Possible Causes : IV too low, Preform too hot, Low level crystallinity in preform
Problem : Pearlescence
Possible Causes : Preform too cold, Insufficient soak time, Improper preform design
Problem : Pearlescence in a Particular Section
Possible Cause : Affected section too cool
Problem : Thin Sidewalls
Possible Causes : Preform too hot, IV too low, excessive preform moisture, improper heating profile
Problem : Heavy neck area
Possible Causes : Preform too hot, IV too low, excessive preform moisture, improper heating profile, too much heat in bottom area, pre-blow air starting too early
Problem : Shelf life failure
Possible Causes : Preform too hot, IV too low, Excessive preform moisture, Improper heating profile
Problem : Heavy bottom area
Possible Causes : Preform too hot, IV too low, Excessive preform moisture, Improper heating profile, Too much heat in top area, pre-blow air starting too late
Problem : Drop Test Failure
Possible Causes : Preform too hot, IV too low, Excessive preform moisture, Improper heating profile, Too much heat in top area, Preblow air starting too late, Excessive gate crystallinity in preform
Problem : Top Load Failure
Possible Causes : Preform too hot, IV too low, Excessive preform moisture, Improper heating profile, Too much heat in top area, Preblow air starting too late
Problem : Creep
Possible Causes : Preform too hot, IV too low, Excessive preform moisture.
Problem : Localized Surface Imperfections
Possible Causes : Water in blow air, Contamination, Small un-melts in preforms
FAQ :
1) Q: What's your MOQ?
A: The MOQ depends on the design and production processes of the products.
Normal this product's MOQ is 10000pcs.

2) Q: Can we do printing on the bottles?
A: We can do printing on the bottles as your requirements. And this will require additional charges.

3) Q: How can we choose the shipping way?
A: For the small order,we will suggest you choose the express,such as the DHL,FEDEX,UPS,TNT,etc.
For the larger order,we will suggest you choose by sea.If you are urgent,you can choose by air.

4) Q: Do you offer the free samples,how can we get the samples?
A: Yes,we would like to supply free samples to you, you just need to pay the sample delivery charge.
We will arrange delivery samples by the DHL,FEDEX,UPS,TNT,etc.

5) Q: Can we combine many items assorted in one container in my first order?
A: Surely as long as each item reach our MOQ.

6) Q: How do you control the preforms quality before shipping the bottles to us?
A: We have the proffesional QC department, and we at least make the 3 times leak test.
Furthermore, we have SGS, CQM and CQC certification.