Wood Veneer Door Skin, Cherry Door Skin, Red Wood Door Skin manufacturer / supplier in China, offering Melamine HDF Door Skin/ Black Walnut MDF Door Skin/ EV Walnut MDF Door Skin for 2.7/ 3.0/4.2mm, New Color Melamine MDF for Decoration or Building Material, Nigeria Market Popular Melamine MDF for Furniture and so on.
Min. Order / Reference FOB Price | |
---|---|
6000 Meter | US $0.05/ Meter |
Local Area: | Weifang, Shandong, China |
---|---|
R&D Capacity: | OEM, ODM, Other |
Payment Terms: | LC, T/T, PayPal |
Customized: | Customized |
---|---|
Certification: | ISO9001 |
Material: | PVC |
MaterialPVC, ABS, Acrylic, Melamine paper, environment friendly materials according to your requirement etcThickness0.4mm - 5mm, Customized sizes can be organizedWidth9mm - 80mm, Customized sizes can be organizedLength(Per Roll)50m, 100m, 200m, 300mSurface ColorTitanium White, Wood Grain, Solid Color, Shine, Glossy, Embossed etc. (Any design/color is available.)FinishHigh Glossy, Bright, Matt, Super Matt, TexturedApplicationFurniture Parts, Furniture Accessories, kitchen cabinet, table, teaching equipment, laboratory, interior design and other construction decorationsTemperatureHigh temperature and low temperature resistantFeaturesNon-color variation after trimming and polishingStrong bonding strengthSuperior durability and wearabilityExcellent light stabilityStain and chemical resistanceHeavy metal freePhthalates freeNo pressure whiteningPackagingProtected with plastic foam and packaged in cartonSupply ability9000,000m per monthMOQ400 MetersShipping Date15 days after receiving the advance payment or L/CPayment TermsTT or L/C at sight
PVC edge banding is divided into several proportions according to the ratio of added PVC and calcium carbonate.
When the proportion of calcium carbonate is high, the physical properties are unstable, the PCV edge banding will be easily broken and fade color. High-quality PVC edge banding, due to the high proportion of PVC components, product stability is very high, then it will not be easily broken and fade color.
The quality of PVC edge banding is generally reflected in the following aspects:
1. The surface is smooth, no bubbles, no lines, and the gloss is moderate;
2. The surface and back are flat, uniform in thickness and uniform in width;
3. The hardness is reasonable, the higher the elasticity, the better the quality and the stronger the wear resistance;
4. The back treatment agent is transparent or white, and The coating should be uniform. If it is not handled properly, it will result in low adhesion and even unable to be bonded after the edge banding;
5. The color of each batch of edge banding should be as consistent as possible.
The smaller the color difference of different batches, the better the quality;
6. No debris and gaps while trimming and cutting
1. Mostly, the higher the temperature, the better the bond strength. It is recommended to use medium and high temperature hot melt adhesive as much as possible for best results.
2. Manual edge banding machine or semi-automatic edge banding machine are not recommended , because there is no polishing function, it is recommended to manually polish to ensure the trimming effect.
3. During the process of use, if the glue line is too thick or there is overflowing and drawing, it is necessary to adjust the speed of the edge banding machine and the temperature of the hot melt adhesive.
4. If the surface of the edge banding tape is easily scratched by the equipment during the edge sealing process, the surface of the edge banding tape is not properly treated and is unqualified.