Tungsten High density alloy
Tungsten Alloy Code: GMW
Density: (17-18.5) g/cm3
Main Component: W(88-98)% with the addition of nickel and copper or nickel and iron, etc.
Main Application:
1-Shakers in micromotor widely used in toys and mobile phones.
2-Radioshielding materials. For example, collimator in flaw detector and clinical Radioshielding needle.
3-Parts of balance wight
4-Widely used in military equipment and fishing equipment to raplace uranium and plumbum for no pollution in circumstance.
5-Used in electro-forge and electro-heading.
6-Used in armor-piercer.
7-Contacts material in high voltage.
8-Inertia balance weight ball in missile, plane and race-car.
Advantages:
-High density
-Excellent mechanical properties such as high vibration-damping capacity and high Young's modulus.
-Excellent radiation-shielding property
-High thermal conductivity with low thermal expansion coefficient
-Higher high-temperature strength and thermal shock resistance
-High oxidation resistance and corrosion resistance
**We supply this material as per customerized sizes and properties.
Typical Properties* HD 17
90% W
6% Ni
4% CuHD 17D
90% W
7% Ni
3% FeHD 17.5
92.5% W
5.25% Ni
2.25% FeHD 17.6
92.5% W
Balance
Ni Fe MoHD 17.7
93% W
Balance
Ni Fe MoHD 18
95% W
3.5% Ni
1.5% CuHD 18D
95% W
3.5% Ni
1.5% FeHD 18.5
97% W
2.1% Ni
.9% FeMill, Spec. T-21014 D
SAE Aero. Materal
Spec. (AMS) 7725C
ASTM-B-777-97Class 1
Type 1
Class 1Class 1
Type 2
Class 1Class 2
----
Class 2Diemitech
----
----S Chat. Free
----
----Class 3
----
Class 3Class 3
----
Class 3Class 4
----
Class 4Density Gms/cc
Density Lbs/cu. in.17
.61417
.61417.5
.63217.6
.63617.7
.63918
.65018
.65018.5
.668Hardness Rockwell C2425263032272728Ultimate Tensile Strength (PSI)110,000120,000114,000120,000125,000110,000120,000123,000Yeild Strength
.2% offset (PSI)80,00088,00084,00090,00095,00085,00090,00085,000Elongation (% in 1")610744775Proportional Elastic
Limit (PSI)45,00052,00046,00055,00060,00045,00044,00045,000Modules of
Elasticity (PSI)40 x 10 645 x 10 647 x 10 652 x 10 653 x 10 645 x 10 650 x 10 653 x 10 6Coefficient of
Thermal Expansion
x 10 -6 / o C (20-400 o C)5.44.614.624.54.54.434.64.5Thermal Conductivity
(CGS Units).23.18.20.27.27.33.26.30Electrical
Conductivity
(% IACS)1410131414161317Magnetic PropertiesNILSlightly MagneticSlightly MagneticSlightly MagneticSlightly MagneticNILSlightly MagneticSlightly Magnetic* Properties may vary according to size and shap of part.
** Composition shown is typical and may change for manufacturing purposes or to meet physical and/or application requirements.
If non-magnetic material is required, it should be specified.