SpecificationsRaction ratio fro Polyol and isocyanateI:P=1.2~1.4Temperture25 degree ClesuisCream time7~13 SGel time30~45 SFree rise density24~27kg/m3Final foam density38~45kg/m3Compress strength>180KPaAdhension strength>160KPaThe stabalityof dimension, -30 degree celsuis, 48h<1.0%Innitial thermal conductivity<0.023w/m.kThe specifications can be adjusted according to the different process of customers.
The blowing agent for blend polyol can be HCFC-141b, water, HFC-245fa and cyclopentane(C5), which is related to the regulations of environment protection in customer's country.Factory overview